I have a customer that the last ice storm we had I used quad release to help
melt the ice on his concrete drive, put down according to manufactor's
specs about 3 lbs. per 500 sq. ft, now since we have had very warm unseasonal weather the drive is starting to crumble very badly. The landscape
supply saleman whom I bought the stuff from said this was caused by the
rapid thawing and freezing of the ice at the time of application if so then why is still coming apart ? and what other advise could ya'll offer me ?
This a very good customer and has gotten me plenty of jobs over the yrs.
he is not blaming me, but is not satisfied at all !!!!! need some help !!!!
Thanks,
melt the ice on his concrete drive, put down according to manufactor's
specs about 3 lbs. per 500 sq. ft, now since we have had very warm unseasonal weather the drive is starting to crumble very badly. The landscape
supply saleman whom I bought the stuff from said this was caused by the
rapid thawing and freezing of the ice at the time of application if so then why is still coming apart ? and what other advise could ya'll offer me ?
This a very good customer and has gotten me plenty of jobs over the yrs.
he is not blaming me, but is not satisfied at all !!!!! need some help !!!!
Thanks,